BB ....your feed rate is too slow if you are producing a "blob" on the end ...it should look like it is "spraying" like disappearing from the end of the wire and re-appearing at the pool surface..... welding the way you are at the moment will not be precise and vertical/overhead welds will just "drop off".....just my 2 penneth.