Only PPE I'm using is gloves, disposable mask and safety glasses, not mixing it with anything just applying to the chassis straight from the tin with a brush.
One of the guys in work used the same stuff on his MG 2 weeks ago and applied it to bare metal (with no primer) and the stuff has gone off solid in 48 hrs...
I'll give it a go on a small area first to see how it goes, I'll give it a week, if it doesn't cure then I'll rethink my plans
I would adopt the option Robo has suggested but I don't have the real estate or equipment to do 2 PK spray so I'm comprising with chassis paint
|