Default Welding with Argon/CO2 vs CO2

I recently bought a bottle of argon/co2 mix of the bay as there wasn't any pure co2 going at the time. It's the 1st time I've used it and it seems to affect the power settings compared to co2? On my normal setting (3/6 power, 4.5 speed) it almost seemed really hot and about to blow holes and looked sounded the same as when i was using co2 on 6/6 power with 5 speed for really thick plate?
Reply With Quote
 


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT +1. The time now is 08:45 AM.


Powered by vBulletin® Version 3.6.4
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.