CTWV50 |
12th February 2015 06:42 PM |
Quote:
Originally Posted by Stot
(Post 99888)
I just figured 200whp would overcome my 1.6 diff in short order so I better get all the 1.8 bits for the exchange.
Cheers
Stot
|
I just wanted a bit more predictability and traction.
So here are the casing parts and flange all cleaned and painted ready for rebuilding.
I cleaned off the calcification on the aluminium case by immersing it in 18 litres of Tesco "cheapo diabetes rot you teeth coke" (£4.95) and used a fish tank water heater in the hope of aiding the process along.
I could of had it bead blasted but I was interested to see if this worked. :D Took the best part of a week but didn't have to scrub at it at all.
I cleaned up the cast iron with electrolysis which as always worked brilliantly. Just a jet wash and blow dry and it was ready for paint.
I bought a external 7-8" micrometer off ebay and I have calibrated it with a 12" digital micrometer today. I'm following this guide for setup of the new diff side bearings.
http://www.miata.net/garage/diff_rr.html
|