Cheers Ronnie....did consider chrome, but too many nasty chemicals involved to get it spot on.... nickel baths you can even put your hand in (dropped a tube in once had to fish it out) as long as you wash it straight away. Gateros plating and caswell do the best kits but as I discovered the most important ability is to be able to control the dc volts and current.
|