You need to use expanded polyurethane foam either the blue or pink stuff with polyester glass gel other wise polyester gel will melt polystrene the common white stuff. I use a timber panel saw and a hand rasp to shape the foam it's easy enough just makes a mes.
Isn't the pink and blue stuff extruded thought the white was the expanded