Default Body Panel Thickness

What type (thickness and grade) and have you guys used for the bodywork aluminium. I want to go with the thinnest practical, not for weight, just for ease of cutting and profiling. But don't want to go so thin its going to dent and crease easy. I assume most people have gone with a 1.5mm 1000 series or similar?
Reply With Quote
  #2  
Old 24th September 2009, 11:20 AM
chriseyj chriseyj is offline
Senior Member
 
Join Date: Feb 2009
Location: Derbyshire
Posts: 121
Default

I've read of some people using 1.2mm for bodywork in a previous. I remember someone mentioning they used a harder grade to usual and found it harder work to shape. Guess it would be more dent resistant though.

Have you any idea of the weight difference between alluminium and fibre glass bodied cars?

Last edited by chriseyj : 24th September 2009 at 11:22 AM.
Reply With Quote
  #3  
Old 24th September 2009, 04:36 PM
thwang thwang is offline
Member
 
Join Date: Sep 2008
Posts: 84
Default

al 1050 semi hard 1.2mm
Reply With Quote
  #4  
Old 24th September 2009, 04:46 PM
deezee's Avatar
deezee deezee is offline
Senior Member
 
Join Date: Jan 2009
Location: Wirral
Posts: 744
Default

I've ordered some 1mm 1050 T14 from Aalco. I'll use it on the cockpit panels and the dash / footwell area. If it seems ok I might try it on body panels, or change thickness and grade.
Reply With Quote
  #5  
Old 24th September 2009, 06:30 PM
fabbyglass
 
Posts: n/a
Default

I used to use NS4 for floor, sides and tunnel then sc1 which is softer to do the rear tub section..but had good few "sleeps" since then
Reply With Quote
  #6  
Old 24th September 2009, 06:51 PM
AshG's Avatar
AshG AshG is offline
Super Moderator
 
Join Date: Jul 2008
Location: Rochester
Posts: 1,882
Default

i used 1.5mm 5000 grade. was pretty hard to work with but the result come out pretty nice.

id i were to do it again i would do the floor with the same stuff but the back and sides with 1mm softer stuff.
Reply With Quote
  #7  
Old 10th November 2009, 03:23 PM
axle's Avatar
axle axle is offline
Senior Member
 
Join Date: Jun 2007
Posts: 226
Default

I am going for the 1.2mm it is really good to work with!
__________________
Regards Axle
Reply With Quote
  #8  
Old 10th November 2009, 04:55 PM
Bonzo's Avatar
Bonzo Bonzo is offline
Senior Member
 
Join Date: Jul 2007
Location: Cornwall
Posts: 3,321
Default

Me too Axle.

1.2mm Semi hard for the sides & rear

Treated myself to a 2mm sheet of Semi hard for the floor & should have enough left over to do the fuel tank.

Really looking forward to playing with the ac tig welder again
__________________
I am not a complete idiot...........Some of the parts are missing !!
Ronnie

www.roadster-builders.co.uk
Reply With Quote
  #9  
Old 11th November 2009, 11:06 AM
Tilly819 Tilly819 is offline
Senior Member
 
Join Date: Oct 2008
Location: Leicestershire
Posts: 489
Default

Hi all,
i used
0.9mm 1050 for the sides
0.9mm L163 for the rear tub, seat back and TT sides
0.9mm L166 fir the bits between the sides and the back with the RAd on then... regret that was a pig to work
1.7mm L163 for the floor

The rest is GRP or will be when iv done the scoop and bonnet mould

Tilly
Reply With Quote
Reply


Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

vB code is On
Smilies are On
[IMG] code is On
HTML code is Off
Forum Jump


All times are GMT +1. The time now is 07:44 AM.


Powered by vBulletin® Version 3.6.4
Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.