#1
|
|||
|
|||
hi
is the 1050a half hard or semi hard we use a lot of half hard at work which is very soft. thwang |
#2
|
||||
|
||||
Lifted this from CKC mag
Grade Properties 1xxx excellent formability,weldability & corrosion resistance.low strength 2xxx excellent machinability & high strength.poor formability,weldability & corrosion resistance 3xxx formable,corrosion resistant & weldable.moderate strength 4xxx formable,weldable,corrosion resistant 5xxx formable,weldable,excellent corrosion resistantance 6xxx good formability,weldability & corrosion resistance.medium strength,heat treatable 7xxx machinable with high strength.poor corrosion resistance & weldability 8xxx excellent formability |
#3
|
||||
|
||||
i used 5251 1.5mm for everything on my car because it happened to be on offer at parkers the week i ordered it. it was a git to bend and shape use 1.2mm 1050 for anything that need a bend in it
__________________
My Roadster Is Finished NerNer....... Pigs can fly, you just have to carry them onto the plane. My Pictures http://s707.photobucket.com/user/ashgardiner/profile/ |
Thread Tools | |
Display Modes | |
|
|